Crushed EPDM

Crushed EPDM

Physical Properties
  • Remove
  • Density
  •  Hardness, Durometer Shore 00
  •  Compression Deflection (25%)(3/8" or 9.53 mm & higher
  •  50% Compression Set (Room Temp)
  •  Tensile Strength
  •  Tear Strength
  •  Elongation
  •  Service Temperature (1)
  •       Low
  •       High Continuous
  •       High Intermittent
  •  Water Absorbtion
  •        Maximum Weight Change
  • Fluid Immersion (7 days at 23°C [73.4°])
  •        ASTM Ref. Fuel B, Weight Change%
  • Accelerated Aging (7 days at 70°C [158°F]
  •       Flexibility (180° bend without cracking)
  •       Appearance change
  •       Change in Compression Deflection
  •  Combustion Characteristics (3)
  • FMVSS-302
  • UL-94
  •        5VA
  •        V-0
  •       HF - 1
Unit
  • Remove
  • kg/m 3
  • lb/ft 3
  •  kPa
  • psi
  •  %
  •  psi
  •  kN/m
  •  ib/in
  • °F (°C)
Test Method
  • Remove
  •  ASTM D 1056
  •  ASTM D 2240
  •  ASTM D 412 (DIE A)
  •  ASTM D 624 (DIE C)
  •  ASTM D 746
  •  Thicknesses
  •  0.125" (3.1 mm) & higher
  •  0.169" - 0.183" (4.29mm - 4.64mm)
  •  0.124" - 0.134" (3.14 mm - 3.41mm)
  •  0.133" - 0.144" (3.37 mm - 3.65mm)
Typical Results
  • Remove
  •  64 - 128
  •  4.0 - 8.0
  •  5 ± 5
  •  6.9 maximum
  •  1.0 maximum
  •  < = 25%
  •  105 minimum
  •  15 minimum
  •  0.7 Typical
  •  4.0 Typical
  •  175 minimum
  •  -70°F (-56°C)
  •  --
  •  250°F (121°C)
  •  Not Applicable
  •  Pass
  •  None
  •  ± 30%
  •  Comments
  •  Listed, UL file #QMFZ2.E55798
Reset filters
Density kg/m 3  ASTM D 1056  64 - 128
Crushed EPDM sponge rubber
Get Quote
lb/ft 3  ASTM D 1056  4.0 - 8.0
Crushed EPDM sponge rubber
Get Quote
 Hardness, Durometer Shore 00  ASTM D 2240  5 ± 5
Crushed EPDM sponge rubber
Get Quote
 Compression Deflection (25%)(3/8" or 9.53 mm & higher  kPa  ASTM D 1056  6.9 maximum
Crushed EPDM sponge rubber
Get Quote
psi  ASTM D 1056  1.0 maximum
Crushed EPDM sponge rubber
Get Quote
 50% Compression Set (Room Temp)  %  ASTM D 1056  < = 25%
Crushed EPDM sponge rubber
Get Quote
 Tensile Strength  kPa  ASTM D 412 (DIE A)  105 minimum
Crushed EPDM sponge rubber
Get Quote
 psi  ASTM D 412 (DIE A)  15 minimum
Crushed EPDM sponge rubber
Get Quote
 Tear Strength  kN/m  ASTM D 624 (DIE C)  0.7 Typical
Crushed EPDM sponge rubber
Get Quote
 ib/in  ASTM D 624 (DIE C)  4.0 Typical
Crushed EPDM sponge rubber
Get Quote
 Elongation  %  ASTM D 412 (DIE A)  175 minimum
Crushed EPDM sponge rubber
Get Quote
 Service Temperature (1)
Crushed EPDM sponge rubber
Get Quote
      Low °F (°C)  ASTM D 746  -70°F (-56°C)
Crushed EPDM sponge rubber
Get Quote
      High Continuous °F (°C)  ASTM D 746  --
Crushed EPDM sponge rubber
Get Quote
      High Intermittent °F (°C)  ASTM D 746  250°F (121°C)
Crushed EPDM sponge rubber
Get Quote
 Water Absorbtion
Crushed EPDM sponge rubber
Get Quote
       Maximum Weight Change  %  ASTM D 1056  Not Applicable
Crushed EPDM sponge rubber
Get Quote
Fluid Immersion (7 days at 23°C [73.4°])
Crushed EPDM sponge rubber
Get Quote
       ASTM Ref. Fuel B, Weight Change%  %  ASTM D 1056  Not Applicable
Crushed EPDM sponge rubber
Get Quote
Accelerated Aging (7 days at 70°C [158°F]
Crushed EPDM sponge rubber
Get Quote
      Flexibility (180° bend without cracking)  ASTM D 1056  Pass
Crushed EPDM sponge rubber
Get Quote
      Appearance change  ASTM D 1056  None
Crushed EPDM sponge rubber
Get Quote
      Change in Compression Deflection  %  ASTM D 1056  ± 30%
Crushed EPDM sponge rubber
Get Quote
 Combustion Characteristics (3)  Thicknesses  Comments
Crushed EPDM sponge rubber
Get Quote
FMVSS-302  0.125" (3.1 mm) & higher  Pass
Crushed EPDM sponge rubber
Get Quote
UL-94
Crushed EPDM sponge rubber
Get Quote
       5VA  0.169" - 0.183" (4.29mm - 4.64mm)  Listed, UL file #QMFZ2.E55798
Crushed EPDM sponge rubber
Get Quote
       V-0  0.124" - 0.134" (3.14 mm - 3.41mm)  Listed, UL file #QMFZ2.E55798
Crushed EPDM sponge rubber
Get Quote
      HF - 1  0.133" - 0.144" (3.37 mm - 3.65mm)  Listed, UL file #QMFZ2.E55798
Crushed EPDM sponge rubber
Get Quote

Quote Cart